If the skins have been dried by a modern drying system they all come out in a uniform condition, and are ready to go on immediately to the next operation. If, however, a form of the "loft" method of drying has been used, it is customary to subject the skins to an additional process. The dried pelts are put in drums with damp sawdust, and drummed for a short time in order to get them into the proper condition. The drumming is essential for the purpose of equalizing the condition of the pelts, some being drier than others, and as a consequence of the contact with the moist sawdust, they are all brought to the same degree of dryness. As a result of this operation also, the skins become considerably softened.
[Illustration: FIG. 12. DELIVERY END OF CONVEYOR DRYER.
(_Proctor & Schwartz, Inc., Philadelphia._)]
Then if the pelts have not been previously oiled during the tanning process, or prior to the drying, they receive this treatment now. The oil or fat is applied to the leather side of the furs, which are then placed in the tramping machine for a short time in order to cause the oil to be forced into the skin. The fibres of the corium thus become coated with a thin layer of fatty material, which contributes greatly to the softness and flexibility of the pelt, and increases its resistance to the action of water, and also, in certain instances a partial chamois tan is produced, thereby improving the quality of the leather.
[Illustration: FIG. 13. STRETCHING MACHINE FOR CASED SKINS.
(_Reliable Machine Works, Evergreen, L. I._)]
The skins are now returned to the work bench, and subjected to the stretching or "staking" process. This consists in drawing the skin in all directions over the edge of a dull blade, which is usually fixed upright in a post with the edge up. Or, the stretching may be done on the fleshing bench, substituting a dull blade for the fleshing knife. Recently staking machines are being used in the larger establishments, the work being done much more quickly and efficiently. As a result of this operation, the leather becomes very soft and flexible, every bit of hardness and stiffness being eliminated, and the skins receive their maximum stretch, thereby giving the greatest possible surface to the pelage. This not only helps to bring out the beauty of the hair, but is also a decided advantage from the economic point of view, as a considerable saving of material is effected in this way, sometimes even to the extent of twenty-five per cent. Cased skins are stretched in a somewhat different manner, by means of stretching irons. These consist of two long iron rods joined by a pivot at one end. The skins are slipped on to the irons, which are then spread apart, and in this way the skins are stretched and softened. A machine which does this work very efficiently is shown in Fig. 13. The skin is drawn onto the stretching arms, in this case made of bronze, which are then forced apart by pressing on a pedal. When properly stretched to the maximum width in all directions possible, and thus thoroughly softened, the skin can easily be reversed, that is, turned hair-side out. As many as 6000 skins can be stretched, or 4000 to 5000 skins stretched and reversed by one man in one day on such a machine.