=Mending.= The object of darning or mending is to make all repairs in the structure of the cloth before the process of fulling. The mender must have a good eye for colors necessary to produce various effects and for the interlacing of the threads. More exact work is required for threadbare fabrics that require little if any finishing afterward, than in dealing with a face finish fabric, where the nap is to be raised and will cover many imperfections so that they will never be noticed in the finished cloth.
=Fulling.= The object of fulling is to render woolen and worsted goods stronger and firmer in body. Fulling is similar to felting, the principal object of each being to condense the fibers, thereby increasing the firmness. Certain varieties of woolens are fulled nearly one-half their original width and length. The process of fulling includes three steps: cleansing, scouring, and condensing the fibers of the cloth. The object of scouring is to get rid of oil used preparatory to spinning, and to remove from the cloth stains and the sizing used in dressing the warp. The cloth is first saturated with hot water and soap, and is then scoured and rubbed between the slow-revolving rollers of the machine from two to eighteen hours, according to the character of goods and the amount of shrinkage desired. The more prolonged the operation, the more the material shrinks. When sufficiently fulled, the length of cloth is scoured to free it from soap. This is done with water, warmed at first, but gradually cooled, until at the end the cloth is worked in cold water. Next the cloth is stretched uniformly in all directions, so that it may dry evenly without wrinkles or curls. Sometimes the cloth is placed in a hot-air chamber to hasten the drying. The fulling or shrinking is effected by the application of moisture, heat, and pressure. Every one is familiar with the fact that woolen blankets, flannels, and hosiery tend to contract with frequent washings, gaining in thickness and solidity what they lose in elasticity. Such shrinkage is greatly hastened when they are rubbed vigorously in hot water and then allowed to cool suddenly. This change is due to the physical properties of the wool fiber.