3. =Blue Bottoming.= The next operation is to dye the silk blue, which is done by immersing it in a solution of potash. In this it is worked for half an hour, when it acquires a deep blue color. It is then taken out, and after rinsing is ready for the "weighting" operations.
4. ="Weighting" Bath.= A catechu bath is now prepared, in which the silk is entered and worked for an hour, and then allowed to steep over night. The result is that the blue on the silk is decomposed, and the goods by absorbing the tannin in the catechu increase in weight from 35 to 40 per cent. This bath is the most important one in the dyeing of "weighted" black silks, as the dyer can regulate the strength of the bath by the addition of tin crystals so as to increase the weight of the silk to an astonishing degree. The proportion of tin crystals used is regulated by the number of iron baths that have previously been given the silk; if two baths of iron have been given, 5 per cent of tin crystals are used; if four baths, 10 per cent, and so on. The action of these chemicals is somewhat complex. All that is known is that by reason of some peculiar quality possessed by silk it is enabled to combine with iron and tin, and that exposure to the air after the baths fixes these chemicals permanently upon the fibers, thus increasing their weight to almost any desired extent. Silk, according to its quality and weight, will take up of these substances from 50 to 200 per cent without creating much suspicion. Instances have been known in which silk has been increased nine times its own weight. All the operations thus far have had for their object the weighting of the silk, although the blueing and the catechu baths have some influence on the finished result. After these come the dyeing operations proper, two in number, mordanting and dyeing.
5. =Mordanting.= A bath of iron liquor heated to 130 degrees F. is provided. The silk is entered, worked well for one hour, then wrung out and hung up to "age" for two hours, after which it is ready for the logwood dye.
6. =Dyeing.= A bath of logwood liquor is prepared to which is added 10 per cent of fustic, and the solution is brought to a temperature of 150 degrees F. In this the silk is entered and worked for an hour, then taken out and wrung dry. Sometimes the black does not come up full enough, and in such cases the bath is repeated.