Anodic bonding is a wafer bonding process to seal glass to either silicon or metal without introducing an intermediate layer; it is commonly used to seal glass to silicon wafers in electronics and microfluidics. This bonding technique, also known as field assisted bonding or electrostatic sealing, is mostly used for connecting silicon/glass and metal/glass through electric fields. The requirements for anodic bonding are clean and even wafer surfaces and atomic contact between the bonding substrates through a sufficiently powerful electrostatic field. Also necessary is the use of borosilicate glass containing a high concentration of alkali ions. The coefficient of thermal expansion (CTE) of the processed glass needs to be similar to those of the bonding partner.
Anodic bonding can be applied with glass wafers at temperatures of 250 to 400 °C or with sputtered glass at 400 °C. Structured borosilicate glass layers may also be deposited by plasma-assisted e-beam evaporation.
This procedure is mostly used for hermetic encapsulation of micro-mechanical silicon elements. The glass substrate encapsulation protects from environmental influences, e.g. humidity or contamination. Further, other materials are used for anodic bonding with silicon, i.e. low-temperature cofired ceramics (LTCC).
Overview
Anodic bonding on silicon substrates is divided into bonding using a thin sheet of glass (a wafer) or a glass layer that is deposited onto the silicon using a technique such as sputtering. The glass wafer is often sodium-containing Borofloat or Pyrex glasses. With an intermediate glass layer, it is also possible to connect two silicon wafers. The glass layers are deposited by sputtering, spin-on of a glass solution or vapor deposition upon the processed silicon wafer. The thickness of these layers range from one to a few micrometers with spin-on glass layers needing 1 µm or less. Hermetic seals of silicon to glass using an aluminum layer with thickness of 50 to 100 nm can reach strengths of 18.0 MPa. This method enables burying electrically isolated conductors in the interface. Bonding of thermally oxidized wafers without a glass layer is also possible.
The procedural steps of anodic bonding are divided into the following:
Contact substrates
Heating up substrates
Bonding by the application of an electrostatic field
Cooling down the wafer stack
with a process characterized by the following variables:
bond voltage UB
bond temperature TB
current limitation IB
The typical bond strength is between 10 and 20 MPa according to pull tests, higher than the fracture strength of glass.
Differing coefficients of thermal expansion pose challenges for anodic bonding. Excessive mismatch can harm the bond through intrinsic material tensions and cause disruptions in the bonding materials. The use of sodium-containing glasses, e.g. Borofloat or Pyrex, serve to reduce the mismatch. These glasses have a similar CTE to silicon in the range of applied temperature, commonly up to 400 °C.
History
Anodic bonding is first mentioned by Wallis and Pomerantz in 1969. It is applied as bonding of silicon wafers to sodium containing glass wafers under the influence of an applied electric field. This method is used up to date as encapsulation of sensors with electrically conducted glasses.
Procedural steps of anodic bonding
Pretreatment of the substrates
The anodic bonding procedure is able to bond hydrophilic and hydrophobic silicon surfaces equally effectively. The roughness of the surface should be less than 10 nm and free of contamination on the surface for the procedure to work properly. Even though anodic bonding is relatively tolerant to contaminations, a widely established cleaning procedure RCA takes place to remove any surface impurities.
The glass wafer can also be chemically etched or powder blasted for creating small cavities, where MEMS devices can be accommodated.
Further mechanisms supporting the bonding process of not completely inert anodic materials can be the planarization or polishing of surfaces and the ablation of the surface layer by electrochemical etching.
Contact the substrates
The wafers that meet the requirements are put into atomic contact. As soon as contact is first established, the bonding process starts close to the cathode and spreads in fronts to the edges, the process taking several minutes. The anodic bonding procedure is based on a glass wafer that is usually placed above a silicon wafer. An electrode is in contact with the glass wafer either through a needle or a full area cathode electrode.